The workshop of WXIT is divided into several areas used for raw material warehousing, raw material detection, numerical control processing, assembly, finished product detection and finished product warehousing. The quality of each step, from raw materials, parts processing, equipment assembly to finished product inspection, is fully guaranteed.
The pressure free sintered silicon carbide has the following characteristics::1.High thermal conductivity:
The thermal conductivity of the pressure free sintered silicon carbide is much higher than other corrosion resistant materials The pressure free sintered silicon carbide occupies a smaller heat transfer area with the same heat exchange efficiency This material allows for a smaller heat exchanger size The pressure free sintered silicon carbide significantly reduces occupied space, which saves money.2. Anti-corrosion:
This material features a high corrosion, oxidation and erosion resistance. The pressure free sintered silicon carbide can withstand high concentrations of sulfuric acid, nitric acid, phosphoric acid, mixed acid, strong alkali, oxidant, and other highly corrosive materials This material is the only ceramic material that cannot be corroded by hydrofluoric acid. It has an excellent service life. The following are the results of different corrosion resistance levels in different solution:Corrosive medium | Temperature(℃) | Corrosion rate mg/cm2.Y | Corrosion rate mm/Y | |
98%H2SO4 | Sulfuric acid | 100 | 0.98 | 0.0032 |
54%HF | Hydrofluoric acid | 25 | 0.06 | 0.0002 |
50%NaOH | Sodium hydroxide | 100 | 1.25 | 0.0040 |
45%KOH | Potassium hydroxide | 100 | 0.04 | 0.0001 |
70%HNO3 | Nitric acid | 86 | 0.04 | 0.0001 |
37%HCL | Hydrochloric acid | 25 | 0.07 | 0.0002 |
10%HF&HNO3 | Hydrofluoric acid & nitric acid | 25 | 0.05 | 0.0002 |
10%HF&HNO3 | Hydrofluoric acid & nitric acid | 120 | 1.25 | 0.0040 |
3. Excellent thermodynamic properties
High strength and high hardness The pressure free sintered silicon carbide has a high abrasion resistance and anti-penetrant efficiency under high temperature and high pressure conditions. This material allows the medium to pass through at high speeds. It can work normally at 1300 ℃.Detected Items | Detection result |
Volume density | 3.12 g/cm3 |
Bending strength | 400 MPa |
Strength of anti-static pressure | 20 MPa |
Elastic modulus | 410 GPa |
Fracture toughness | 3.80 Mpa*m1/2 |
Heat conductivity(room temperature) | 140 W/m*K |
Coefficient of thermal expansion | 4.66(RT-1000oC)10-6/K |