Product Ingredients
Epoxy resin, chlorosulfonated polyethylene, rubber, coal, asphalt, refinedvegetable oil, organosilicone resin, various rust-proofand anti-corrosion pigment, fillings, additive, solvent, etc.
Usage of Anti-corrosion Paint
Our anti-corrosion paint totally has 9 kinds of products, which areseparately used in the inner wall of gasoline tanks, gas arks, water-proofbuilding coat, protective coat of cooling water tower, steel structure which isused under environment between dry and wet, anti-rust priming, electricityfactories, flues and exterior wall of watercrafts.
Property of Anti-corrosion Paint
This series of products have goodproperty for decoration and anti-corrosion. (Detailed information isattached in the product instruction.)
Paints | Environment condition | Thickness of dry film (micron) | Den -sity | Coating Method | Mixing ratio | Drying Time | No. of Coating | Preserved Life (months) |
| ||||||||||
Chlorosulfonated polyethylene anti-corrosion paints | General coating | 80—100 | 1.12 | Spray-coating brush coating | A : B =10 : 1 | Surface dry: 0.5h inner dry: 24h | 3—4 | 12 |
| ||||||||||
Hydroxy-acid enamel paint | Decorative coating | 100—150 | 1.27 | Spray-coating brush coating | Single component | Surface dry: 6h inner dry: 24h | 2—4 | 12 |
| ||||||||||
Organosilicon high temperature-resistant, anti-corrosion paint | Chemicals-resist-ant atmospheric coating | 100—140 | 1.23 | Spray-coating brush coating | A : B =100 : 2 | Surface dry: 1h inner dry: 24h | 2—3 | 12 |
| ||||||||||
Anti-corrosion paint special for power plant spots | Acid, alkali, and salt-resistant chemistry medium coating | 150—220 | 1.12 | Spray-coating brush coating | A : B =18 : 3 | Surface dry: 2h inner dry: 24h | 2—4 | 12 |
| ||||||||||
Paints for interior finished-oil cans | Waterproof, oil -resistant coating | 140—180 | 1.45 | Spray-coating brush coating | A : B =11 : 15 | Surface dry: 2h inner dry: 24h | 2—3 | 12 |
| ||||||||||
Chlorosulfonated polyethylene anti-crack and anti-corrosion paints | Anti-crack coating | 80—120 | 1.21 | pray-coating brush coating | A : B =10 : 1 | Surface dry: 0.5h inner dry: 24h | 2-3 | 6 |
| ||||||||||
|
|
|
|
|
|
|
|
|
| ||||||||||
|
|
|
|
|
|
|
|
|
| ||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
| |||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Anti-corrosion paints for Epoxy asphalt underground | Ocean moisture -resistant coating | 20——300 | 1.13 | Spray-coating brush coating | A : B =10 : 1 | Surface dry: 2h inner dry: 24h | 2—4 | 12 |
Anti-corrosion paints for gas cabinet | Anti-corrosion coat in gas cabinet | 150—200 | 1.15 | Spray-coating brush coating | A : B =10 : 1 | Surface dry: 0.5h inner dry: 24h | 2—5 | 6 |
Damp-proof paint for Cooling water tower | Cooling water tower interior coat | 150—180 | 1.18 | Spray-coating brush coating | A : B =10 : 1 | Surface dry: 0.5h inner dry: 24h | 2—4 | 6 |