Dispersion unshifted single-mode optical fiber is suitable for wavelengths of 1260nm to 1625nm. It maintains the low dispersion of 1310nm in the traditional band and low loss at 1383nm, which makes full use of the E-band (1360nm ~ 1460nm), and improves the macro-bend resistance of the L-band (1565-1625nm), reducing the bend loss at 1625nm wavelength.
CharacteristicsApplicable to the following optical cable structures: central-tube fiber optical cable, stranded loose tube fiber optical cable, slotted core fiber optical cable, ADSS fiber optical cable, etc.
Technical SpecificationType | Properties | Unit | Value |
Geometrical Specifications | Cladding Diameter | μm | 125±0.7 |
Cladding Non-Circularity | % | ≤1 | |
Coating Diameter | μm | 235-252 | |
Coating Non-Circularity | % | ≤6 | |
Core-Clad Concentricity | μm | ≤0.54 | |
Coating-Clad Concentricity | μm | ≤12 | |
Fiber Curl | m | ≥4 | |
Optical Specifications | 1310nmMFD | μm | 8.2-9 |
1550nmMFD | μm | 9.3-10.3 | |
1310nmAtt | dB/km | 0.31-0.354 | |
1383nmAtt | dB/km | 0.25-0.344 | |
1550nmAtt | dB/km | 0.17-0.214 | |
1625nmAtt | dB/km | 0.18-0.234 | |
1285-1330nm @1310nm | dB/km | ≤0.04 | |
1525-1575nm @1550nm | dB/km | ≤0.02 | |
Terminal Difference at 1310nm | dB/km | ≤0.05 | |
Terminal Difference at 1550nm | dB/km | ≤0.05 | |
Point Discontinuity at 1310nm | dB | ≤0.05 | |
Point Discontinuity at 1550nm | dB | ≤0.05 | |
Uniformity at 1310nm | dB/km (500m) | ≤0.05 | |
Uniformity at 1550nm | dB/km (500m) | ≤0.05 | |
Zero Dispersion Wavelength | nm | 1300-1324 | |
Zero Dispersion Slope | ps/(nm2.km) | 0.08-0.092 | |
PMD | ps/(km1/2) | ≤0.124 | |
1285-1339nm @1310 | ps/(nm.km) | ≤3.4 | |
1271-136nm @1550 | ps/(nm.km) | ≤5.3 | |
Chromatic Dispersion at 1550nm | ps/(nm.km) | 14-18 | |
Chromatic Dispersion at 1625nm | ps/(nm.km) | 18-22 | |
Fiber Cutoff Wavelength | nm | 1150-1330 | |
Cable Cutoff Wavelength | nm | ≤1260 | |
Macro-bend Loss at 1550nm (Ф30mm) | dB | ≤0.03 | |
Macro-bend Loss at 1625nm (Ф30mm) | dB | ≤0.1 | |
Macro-bend Loss at 1550nm (Ф20mm) | dB | ≤0.1 | |
Macro-bend Loss at 1625nm (Ф20mm) | dB | ≤0.2 | |
Macro-bend Loss at 1550nm (Ф15mm) | dB | ≤0.5 | |
Macro-bend Loss at 1625nm (Ф15mm) | dB | ≤1.0 | |
Mechanical Specifications | Proof Test | N | ≥8.5 |
Strip Force (peak) | N | 1.0-8.9 | |
Strip Force (average) | N | 1.0-5.0 | |
Dynamic Tensile Strength (15%) | Gpa | ≥3.05 | |
Dynamic Tensile Strength (50%) | Gpa | ≥3.72 | |
Dynamic Fatigue (Nd) | ≥20 | ||
Environmental Specifications | Temperature Humidity Cycling at 1310nm | dB/km | ≤0.05 |
Temperature Humidity Cycling at 1550nm | dB/km | ≤0.05 | |
Water Immersion at 1310nm | dB/km | ≤0.05 | |
Water Immersion at 1550nm | dB/km | ≤0.05 | |
Damp Heat at 1310nm | dB/km | ≤0.05 | |
Damp Heat at 1550nm | dB/km | ≤0.05 | |
Heat Aging at 1310nm | dB/km | ≤0.05 | |
Heat Aging at 1550nm | dB/km | ≤0.05 |