Features Outstanding resistance to chloride-induced stress corrosion Very good corrosion resistance when in contact with oxidizing and reducing media The combination of molybdenum (approximately 6.5%) and nitrogen (approximately 0.2%) in its composition resists pitting and crevice corrosion Chemical Analysis
| % | Ni | Cr | C | Mn | Fe | Si | Cu | Mo | N | Ti | P | S |
Incoloy 926 | Min. | 24 | 19 | - | - | Balance | - | 0.5 | 6 | 0.15 | 0.6 | - | - |
Max. | 26 | 21 | 0. 02 | 2 | Balance | 0.5 | 1.5 | 7 | 0.25 | 1.2 | 0.03 | 0. 01 |
Physical Properties
Density | 8.1G/CM3 |
Melting Range | 1320-1390°C |
The Min. Mechanical Properties under Room Temperature
Alloy | Tensile Strength | Yield Strength | Elongation |
RM N/MM2 | RPO.2 N/MM2 | A5% |
926 | 650 | 295 | ≤35 |
Applications Seawater environments Heat exchangers, tank housings Distributor systems for sulfuric acid Condenser pipes Pump lines in oil and gas extraction