TIG Welding Wire
Our company produces many kinds of welding wires and this TIG welding wire is specially designed for argon arc welding. This TIG welding wire has mechanical performance and great welding performance. TIG welding wire has advantages of high melting speed, high deposition rate, steady arc and beautiful welding seam.
Furthermore, anti-corrosion ability is very strong and TIG welding wire is not sensitive to air hole in the welding metal. There are C, Mn, Si, P, S, Si, Cu, Ni, Cr, Mo, V, Fe and other elements. Actually the amount of Si is 1.15% and is much bigger than 0.80%. This can prevent the iron in the welding wire from reacting with oxygen and restore FeO. The amount of S is less than 0.025%, and more than 1.85% Mn is added in the welding wire. This ensures that S in the welding wire will be eliminated and leak caused during welding will not occur. And the amount of P is less than 0.025%, so the welding metal has good plastic property and elongation. Then welding metal will not be sensitive to leaks.
Technical Specifications
Specification& Classification : AWSER70S-6 | ||||||||||||||||||||||
Chemical Composition ( % ) | ||||||||||||||||||||||
Elements | C | Mn | Si | P | S | Cu | Ni | Cr | Mo | V | Fe | |||||||||||
Requirement | 0.06 0.15 | 1.40 1.85 | 0.80 1.15 | Max. 0.025 | Max. 0.025 | Max. 0.50 | Max. 0.15 | Max. 0.15 | Max. 0.15 | Max. 0.03 | ﹎ | |||||||||||
Deposited Metal | ﹎ | ﹎ | ﹎ | |||||||||||||||||||
Tensile Test of Deposited Metal | Impact Test of Deposited Metal | |||||||||||||||||||||
Vieldstrength Mpa (σ0.2) | Tensile Strength Mpa (σb ) | Elongation % ( δ5 ) | Test temp ℃ | Absorbed Energy(Akv ) J | ||||||||||||||||||
Requirement | 420Min. | 500Min. | 22 Min. | -30 | 27 | |||||||||||||||||
Test Result | ||||||||||||||||||||||
WE HEREBY CERTIFY THAT THIS REPORT IS CORRECT AND THAT ALL TEST RESULTS ARE IN COMPLIANCE WITH THE SPECIFICATION DESCRIBED HEREIN. QUALITY CONTROL SECTION Liu Zhonghua |