Achieving powder surface modification by changing the cyclone vortex Achieving powder surface modification by changing the cyclone vortex Relative motion of the three rotors modifies the impact of cyclone swirls to coat the powder's surface.
Mature technology requires minimal initial investment, hence making it suitable for stearic acid coating.
Heat generated through self-friction and no additional heat source is required. As a result, the amount of auxiliary equipment and the cost for operation is kept to a minimum.
Suitable for 325 ~ 1250 mesh powder coating.
Power range: 11 kW ~ 225 kW
Maximum output: 6 t/h Technical parameter (calcium carbonate)
Parameter | 300/3 | 600/3 | 900/3 |
Grinding disc rotate speed (rpm) | 5050 | 2580 | 1850 |
Grinding disc linear speed (m/s) | 77.4 | 85.1 | 87.2 |
Grinding disc power (kW) | 3×18.5 | 3×37 | 3×37 |
Max. air flow (m³/h) | 2000 | 6000 | 9000 |
Note: The particle size, specific gravity, hardness, and moisture of raw materials are all closely associated to the production capacity. These parameters should only be used as a reference; for more detailed information please consult our engineers.